Depending on the Aluminum alloy you heat treat it to a T-3 or T-4 condition by taking an O condition up to around 500Deg. F for 30 to 40 min, then water quench. This makes it harder. To Age it to a T-6 condition it goes up to 900 to 1000 deg. for 6 to 10 hours depending again on the alloy, and allow to air cool. This is what I did for 5 years working for McDonnell Douglas in Florida. I never did stainless steel.
__________________
Wanted: Simmons Super Power Head
Craig Likon 1931 150B
ctlikon0712 is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Sponsored Links (Register now to hide all advertisements)


All times are GMT -5. The time now is 06:36 PM.