Looks like your moving along. You mentioned when you where forming the firewall that you had a problem with cracking. What grade of aluminum are you using? And are you annealing the areas where you're doing the shaping? 1000 or 3000 will work nicely for body panels. 5000 can be hard to work with. All of these can be annealed. Hope this helps. JP